商品の詳細:
|
| 結合型: | ピッチボンデッド | 見かけの気孔率: | 5% |
|---|---|---|---|
| MgO含有量: | 79% | かさ密度: | 2.98g/cm3 |
| 冷たい粉砕強度: | 48 MPa | 負荷下の屈折率: | 1660℃ |
| 固定炭素含有量: | 12% | ||
| ハイライト: | C12 Slide Gate Brick,Low Porosity Pocket Block,Sequence Casting Refractory |
||
Produced from dead burnt magnesia with a controlled 12% graphite addition, each C12 brick is pressed to 2.98 g/cm3 and cured under the pitch bond route used for slide gate pocket work in ladle flow control system. The body is pressed in steel moulds to tight dimensional tolerance, then heat treated so the binder cokes evenly through the section. With 5% apparent porosity and 48 MPa cold crushing strength, the brick survives transport, installation and the first heat-up
コンタクトパーソン: Mr. Pika
電話番号: 86-13838387996