商品の詳細:
|
| 結合型: | 樹脂結合 | 見かけの気孔率: | 6% |
|---|---|---|---|
| MgO含有量: | 76% | かさ密度: | 3.01 g/cm3 |
| 冷たい粉砕強度: | 50 MPa | 負荷下の屈折率: | 1680℃ |
| 固定炭素含有量: | 14% | ||
| ハイライト: | C14 Furnace Spout Brick,High Strength Tapping Unit,Electric Furnace Refractory |
||
Produced from dead burnt magnesia with a controlled 14% graphite addition, each C14 brick is pressed to 3.01 g/cm3 and cured under the resin bond route used for furnace tapping spout work in electric melting furnace. The body is pressed in steel moulds to tight dimensional tolerance, then heat treated so the binder cokes evenly through the section. With 6% apparent porosity and 50 MPa cold crushing strength, the brick survives transport, installation and the first heat-up