商品の詳細:
|
| 結合型: | 含浸ピッチ | 見かけの気孔率: | 6% |
|---|---|---|---|
| MgO含有量: | 75% | かさ密度: | 3.01 g/cm3 |
| 冷たい粉砕強度: | 42 Mpa | 負荷下の屈折率: | 1690 ℃ |
| 固定炭素含有量: | 14% | ||
| ハイライト: | C14 AOD Cone Brick,Oxidation Resistant Unit,Decarburization Vessel Lining |
||
For AOD cone section duty in a AOD refining vessel, these C14 bricks combine 75% MgO with 14% carbon and a pitch impregnated matrix that resists spalling during AOD decarburization. Carbon content is held at 14% because that is the level where thermal conductivity, slag wetting and oxidation loss stay in balance for AOD decarburization. Apparent porosity of 6% keeps liquid slag from reaching the brick interior, while a cold crushing strength of 42 MPa supports the mechanical
コンタクトパーソン: Mr. Pika
電話番号: 86-13838387996
ファックス: 86-0371-56010932