商品の詳細:
|
| 結合型: | グラファイト強化 | 見かけの気孔率: | 6% |
|---|---|---|---|
| MgO含有量: | 79% | かさ密度: | 2.99g/cm3 |
| 冷たい粉砕強度: | 43MPa | 負荷下の屈折率: | 1640℃ |
| 固定炭素含有量: | 12% | ||
| ハイライト: | C12 Flash Furnace Brick,Graphite Enhanced Unit,Nickel Smelting Refractory |
||
Produced from dead burnt magnesia with a controlled 12% graphite addition, each C12 brick is pressed to 2.99 g/cm3 and cured under the graphite enhancement route used for nickel flash furnace sidewall work in nickel flash smelting furnace. The body is pressed in steel moulds to tight dimensional tolerance, then heat treated so the binder cokes evenly through the section. With 6% apparent porosity and 43 MPa cold crushing strength, the brick survives transport, installation